DIN EN 12513:2011-05
Founding - Abrasion resistant cast irons; German version EN 12513:2011
| Fecha edición: |
2011-05-01
En Vigor
|
|---|---|
| Idiomas disponibles: | Inglés, Alemán |
| Resumen: | This European Standard defines the grades of abrasion resistant white cast irons. It also specifies the grades in terms of: - chemical composition - hardness. The types of abrasion resistant white cast irons covered by this standard are: a) unalloyed or low cast irons; b) nickel chromium cast irons covering two general types: - 4 % Ni and 2 % Cr cast irons; - 9 % Cr and 5 % Ni cast irons; c) high chromium cast irons covering four ranges of chromium content. This European Standard does not define the abrasion resistant grades of ausferritic spheroidal graphite cast iron which are subject of EN 1564. |
| Keywords: | Abrasion-resistant materials|Alloys|Castings|Cast-iron|Chemical composition|Chromium content|Classification|Classification systems|Definitions|Foundry practice|Grades|Hardness|Heat treatment|Kind|Materials|Microstructure|Selection of grades|Specification (approval)|Surveys|Wall thicknesses|Wear|Wear resistance |
| ICS: | 77.080.10 - Fundiciones |
| CTN: | |
|
Equivalencia Internacional |
Idéntica EN 12513:2011 |
|
Reemplazo Normas |
Reemplaza a DIN EN 12513:2001-01 Reemplaza a DIN EN 12513:2009-07 |